[{"id":23,"substance":"Hydrogen","phase":"gas","table":"Main","cp_j_per_g_k":14.3,"cp_molar_j_per_mol_k":28.82,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":22,"substance":"Helium","phase":"gas","table":"Main","cp_j_per_g_k":5.193,"cp_molar_j_per_mol_k":20.786,"cv_molar_j_per_mol_k":12.471,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":4,"substance":"Ammonia","phase":"liquid","table":"Main","cp_j_per_g_k":4.7,"cp_molar_j_per_mol_k":80.08,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.26,"cv_per_atom_r":3.21},{"id":29,"substance":"Lithium at 181 °C","phase":"liquid","table":"Main","cp_j_per_g_k":4.379,"cp_molar_j_per_mol_k":30.33,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.242,"cv_per_atom_r":3.65},{"id":28,"substance":"Lithium at 181 °C","phase":"solid(?)","table":"Main","cp_j_per_g_k":4.233,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":50,"substance":"Water at 100 °C","phase":"liquid","table":"Main","cp_j_per_g_k":4.216,"cp_molar_j_per_mol_k":75.95,"cv_molar_j_per_mol_k":67.9,"cp_volumetric_j_per_cm3_k":3.77,"cv_per_atom_r":null},{"id":49,"substance":"Water at 25 °C","phase":"liquid","table":"Main","cp_j_per_g_k":4.181,"cp_molar_j_per_mol_k":75.34,"cv_molar_j_per_mol_k":74.55,"cp_volumetric_j_per_cm3_k":4.138,"cv_per_atom_r":null},{"id":65,"substance":"Water","phase":"liquid","table":"Building materials","cp_j_per_g_k":4.181,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":27,"substance":"Lithium","phase":"solid","table":"Main","cp_j_per_g_k":3.58,"cp_molar_j_per_mol_k":24.8,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.912,"cv_per_atom_r":2.98},{"id":5,"substance":"Animal tissue (incl. human)","phase":"mixed","table":"Main","cp_j_per_g_k":3.5,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.7,"cv_per_atom_r":null},{"id":38,"substance":"Paraffin wax C₂₅H₅₂","phase":"solid","table":"Main","cp_j_per_g_k":2.5,"cp_molar_j_per_mol_k":900,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.325,"cv_per_atom_r":null},{"id":16,"substance":"Ethanol","phase":"liquid","table":"Main","cp_j_per_g_k":2.44,"cp_molar_j_per_mol_k":112,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.925,"cv_per_atom_r":null},{"id":39,"substance":"Polyethylene (rotomolding grade)","phase":"solid","table":"Main","cp_j_per_g_k":2.302,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.15,"cv_per_atom_r":null},{"id":17,"substance":"Gasoline (octane)","phase":"liquid","table":"Main","cp_j_per_g_k":2.22,"cp_molar_j_per_mol_k":228,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.64,"cv_per_atom_r":null},{"id":32,"substance":"Methane at 2 °C","phase":"gas","table":"Main","cp_j_per_g_k":2.191,"cp_molar_j_per_mol_k":35.69,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":33,"substance":"Methanol","phase":"liquid","table":"Main","cp_j_per_g_k":2.14,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":68.62,"cp_volumetric_j_per_cm3_k":1.695,"cv_per_atom_r":null},{"id":51,"substance":"Water at −10 °C (ice)","phase":"solid","table":"Main","cp_j_per_g_k":2.05,"cp_molar_j_per_mol_k":38.09,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.938,"cv_per_atom_r":null},{"id":48,"substance":"Water at 100 °C (steam)","phase":"gas","table":"Main","cp_j_per_g_k":2.03,"cp_molar_j_per_mol_k":36.5,"cv_molar_j_per_mol_k":27.5,"cp_volumetric_j_per_cm3_k":1.53,"cv_per_atom_r":null},{"id":9,"substance":"Beryllium","phase":"solid","table":"Main","cp_j_per_g_k":1.82,"cp_molar_j_per_mol_k":16.4,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.367,"cv_per_atom_r":1.97},{"id":66,"substance":"Wood","phase":"solid","table":"Building materials","cp_j_per_g_k":1.7,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":34,"substance":"Molten salt (142–540 °C)","phase":"liquid","table":"Main","cp_j_per_g_k":1.56,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.62,"cv_per_atom_r":null},{"id":42,"substance":"Sodium","phase":"solid","table":"Main","cp_j_per_g_k":1.23,"cp_molar_j_per_mol_k":28.23,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.19,"cv_per_atom_r":3.39},{"id":61,"substance":"Gypsum","phase":"solid","table":"Building materials","cp_j_per_g_k":1.09,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":35,"substance":"Nitrogen","phase":"gas","table":"Main","cp_j_per_g_k":1.04,"cp_molar_j_per_mol_k":29.12,"cv_molar_j_per_mol_k":20.8,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":36,"substance":"Neon","phase":"gas","table":"Main","cp_j_per_g_k":1.03,"cp_molar_j_per_mol_k":20.786,"cv_molar_j_per_mol_k":12.471,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":30,"substance":"Magnesium","phase":"solid","table":"Main","cp_j_per_g_k":1.02,"cp_molar_j_per_mol_k":24.9,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.773,"cv_per_atom_r":2.99},{"id":24,"substance":"Hydrogen sulfide H₂S","phase":"gas","table":"Main","cp_j_per_g_k":1.015,"cp_molar_j_per_mol_k":34.6,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":2,"substance":"Air (typical room conditions)","phase":"gas","table":"Main","cp_j_per_g_k":1.012,"cp_molar_j_per_mol_k":29.19,"cv_molar_j_per_mol_k":20.85,"cp_volumetric_j_per_cm3_k":0.00121,"cv_per_atom_r":null},{"id":1,"substance":"Air (Sea level, dry, 0 °C (273.15 K))","phase":"gas","table":"Main","cp_j_per_g_k":1.0035,"cp_molar_j_per_mol_k":29.07,"cv_molar_j_per_mol_k":20.764,"cp_volumetric_j_per_cm3_k":0.001297,"cv_per_atom_r":null},{"id":53,"substance":"Asphalt","phase":"solid","table":"Building materials","cp_j_per_g_k":0.92,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":37,"substance":"Oxygen","phase":"gas","table":"Main","cp_j_per_g_k":0.918,"cp_molar_j_per_mol_k":29.38,"cv_molar_j_per_mol_k":21,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":3,"substance":"Aluminium","phase":"solid","table":"Main","cp_j_per_g_k":0.897,"cp_molar_j_per_mol_k":24.2,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.422,"cv_per_atom_r":2.91},{"id":55,"substance":"Concrete","phase":"solid","table":"Building materials","cp_j_per_g_k":0.88,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":62,"substance":"Marble, mica","phase":"solid","table":"Building materials","cp_j_per_g_k":0.88,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":18,"substance":"Glass","phase":"solid","table":"Main","cp_j_per_g_k":0.84,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.1,"cv_per_atom_r":null},{"id":54,"substance":"Brick","phase":"solid","table":"Building materials","cp_j_per_g_k":0.84,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":56,"substance":"Glass, silica","phase":"liquid","table":"Building materials","cp_j_per_g_k":0.84,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":12,"substance":"Carbon dioxide CO₂","phase":"gas","table":"Main","cp_j_per_g_k":0.839,"cp_molar_j_per_mol_k":36.94,"cv_molar_j_per_mol_k":28.46,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":63,"substance":"Sand","phase":"solid","table":"Building materials","cp_j_per_g_k":0.835,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":64,"substance":"Soil","phase":"solid","table":"Building materials","cp_j_per_g_k":0.8,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":20,"substance":"Granite","phase":"solid","table":"Main","cp_j_per_g_k":0.79,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.17,"cv_per_atom_r":null},{"id":60,"substance":"Granite","phase":"solid","table":"Building materials","cp_j_per_g_k":0.79,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":59,"substance":"Glass, borosilicate","phase":"liquid","table":"Building materials","cp_j_per_g_k":0.753,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":21,"substance":"Graphite","phase":"solid","table":"Main","cp_j_per_g_k":0.71,"cp_molar_j_per_mol_k":8.53,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.534,"cv_per_atom_r":1.03},{"id":40,"substance":"Silica (fused)","phase":"solid","table":"Main","cp_j_per_g_k":0.703,"cp_molar_j_per_mol_k":42.2,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.547,"cv_per_atom_r":null},{"id":57,"substance":"Glass, crown","phase":"liquid","table":"Building materials","cp_j_per_g_k":0.67,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":45,"substance":"Titanium","phase":"solid","table":"Main","cp_j_per_g_k":0.523,"cp_molar_j_per_mol_k":26.06,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.638,"cv_per_atom_r":3.13},{"id":7,"substance":"Argon","phase":"gas","table":"Main","cp_j_per_g_k":0.5203,"cp_molar_j_per_mol_k":20.786,"cv_molar_j_per_mol_k":12.471,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":15,"substance":"Diamond","phase":"solid","table":"Main","cp_j_per_g_k":0.509,"cp_molar_j_per_mol_k":6.115,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.782,"cv_per_atom_r":0.74},{"id":58,"substance":"Glass, flint","phase":"liquid","table":"Building materials","cp_j_per_g_k":0.503,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":null,"cv_per_atom_r":null},{"id":43,"substance":"Steel","phase":"solid","table":"Main","cp_j_per_g_k":0.466,"cp_molar_j_per_mol_k":null,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.756,"cv_per_atom_r":null},{"id":13,"substance":"Chromium","phase":"solid","table":"Main","cp_j_per_g_k":0.449,"cp_molar_j_per_mol_k":23.35,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.21,"cv_per_atom_r":2.81},{"id":25,"substance":"Iron","phase":"solid","table":"Main","cp_j_per_g_k":0.449,"cp_molar_j_per_mol_k":25.09,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.537,"cv_per_atom_r":3.02},{"id":52,"substance":"Zinc","phase":"solid","table":"Main","cp_j_per_g_k":0.387,"cp_molar_j_per_mol_k":25.2,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.76,"cv_per_atom_r":3.03},{"id":14,"substance":"Copper","phase":"solid","table":"Main","cp_j_per_g_k":0.385,"cp_molar_j_per_mol_k":24.47,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":3.45,"cv_per_atom_r":2.94},{"id":8,"substance":"Arsenic","phase":"solid","table":"Main","cp_j_per_g_k":0.328,"cp_molar_j_per_mol_k":24.6,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.878,"cv_per_atom_r":2.96},{"id":41,"substance":"Silver","phase":"solid","table":"Main","cp_j_per_g_k":0.233,"cp_molar_j_per_mol_k":24.9,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.44,"cv_per_atom_r":2.99},{"id":11,"substance":"Cadmium","phase":"solid","table":"Main","cp_j_per_g_k":0.231,"cp_molar_j_per_mol_k":26.02,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2,"cv_per_atom_r":3.13},{"id":44,"substance":"Tin","phase":"solid","table":"Main","cp_j_per_g_k":0.227,"cp_molar_j_per_mol_k":27.112,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.659,"cv_per_atom_r":3.26},{"id":6,"substance":"Antimony","phase":"solid","table":"Main","cp_j_per_g_k":0.207,"cp_molar_j_per_mol_k":25.2,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.386,"cv_per_atom_r":3.03},{"id":31,"substance":"Mercury","phase":"liquid","table":"Main","cp_j_per_g_k":0.1395,"cp_molar_j_per_mol_k":27.98,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.888,"cv_per_atom_r":3.36},{"id":46,"substance":"Tungsten","phase":"solid","table":"Main","cp_j_per_g_k":0.134,"cp_molar_j_per_mol_k":24.8,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.58,"cv_per_atom_r":2.98},{"id":19,"substance":"Gold","phase":"solid","table":"Main","cp_j_per_g_k":0.129,"cp_molar_j_per_mol_k":25.42,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.492,"cv_per_atom_r":3.05},{"id":26,"substance":"Lead","phase":"solid","table":"Main","cp_j_per_g_k":0.129,"cp_molar_j_per_mol_k":26.4,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.44,"cv_per_atom_r":3.18},{"id":10,"substance":"Bismuth","phase":"solid","table":"Main","cp_j_per_g_k":0.123,"cp_molar_j_per_mol_k":25.7,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":1.2,"cv_per_atom_r":3.09},{"id":47,"substance":"Uranium","phase":"solid","table":"Main","cp_j_per_g_k":0.116,"cp_molar_j_per_mol_k":27.7,"cv_molar_j_per_mol_k":null,"cp_volumetric_j_per_cm3_k":2.216,"cv_per_atom_r":3.33}]